Material Notes:
General service EPDMInformation provided by Seals Eastern, Inc.
Mechanical Properties Metric English Comments
Hardness, Shore A >= 50
>= 50
ASTM D2240, Type A
53
53
AVG; ASTM D2240, Type A
Tensile Strength at Break >= 6.84 MPa
>= 992 psi
ASTM D412 Method A
9.866 MPa
1431 psi
AVG; ASTM D412 Method A
Tensile Strength, Yield >= 0.607 MPa
>= 88.0 psi
Stress at Elongation M50; ASTM D412 Method A
>= 1.06 MPa
>= 154 psi
Stress at Elongation M100; ASTM D412 Method A
1.10 MPa
159 psi
AVG Stress at Elongation M50; ASTM D412 Method A
1.81 MPa
263 psi
AVG Stress at Elongation M100; ASTM D412 Method A
Elongation at Break >= 363 %
>= 363 %
ASTM D412 Method A
409 %
409 %
AVG; ASTM D412 Method A
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -51.1 °C
-60.0 °F
ASTM D1329
Descriptive Properties Value Comments
Strain Energy / Unit Volume at 20% Elongation (psi) 17