Süd-Chemie Nanofil® 5 Flame Retardant

Category Other Engineering Material , Additive/Filler for Polymer , Polymer
Manufacturer Süd-Chemie
Trade Name Nanofil®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Süd-Chemie Nanofil® 5 Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Standard grades for inorganic flame retardant cable formulations with good pre-dispersibility.Application:PE/EVAGrafted PP Cable formulationAutomotiveTechnical PartsImproves: Abrasion/Scratch Resistance
Physical Properties Metric English Comments
Additive Loading 3.0 - 5.0 %
3.0 - 5.0 %
for Flammability V-0
Melt Flow 1.3 g/10 min

@Load 10.0 kg,
Temperature 190 °C
1.3 g/10 min

@Load 22.0 lb,
Temperature 374 °F
EVA/ATH/Nanofil® 5 (42:55:3)
Mechanical Properties Metric English Comments
Elongation at Break 3.0 %
3.0 %
EVA/ATH/Nanofil® 5 (42:55:3)
Thermal Properties Metric English Comments
Flammability, UL94 V-0
V-0
PE/EVA Sheathing 55% ATH/Mg(OH)2 + 5% Nanofil (recommended)
Descriptive Properties Value Comments
Type Organic intercalated Nanoclay