Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Schott S8801 Contrast Enhancement Filter

Category Ceramic , Glass , Filter
Manufacturer Schott North America
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Schott S8801 Contrast Enhancement Filter.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Contrast Enhancement FilterInformation Provided by SCHOTT North America, Inc.
Physical Properties Metric English Comments
Density 2.64 g/cc
0.0954 lb/in³
Thermal Properties Metric English Comments
CTE, linear 9.10 µm/m-°C

@Temperature 20.0 - 300 °C
5.06 µin/in-°F

@Temperature 68.0 - 572 °F
Transformation Temperature, Tg 538 °C
1000 °F
Softening Point 740 °C
1360 °F
Working Point 1033 °C
1891 °F
Annealing Point 527 °C
981 °F
Strain Point 527 °C
981 °F
Optical Properties Metric English Comments
Refractive Index 1.523
1.523
n<sub>d</sub>, Sodium
Transmission, Visible 55.5 %

@Wavelength 445 nm
55.5 %

@Wavelength 445 nm
86.5 %

@Wavelength 555 nm
86.5 %

@Wavelength 555 nm
90.5 %

@Wavelength 630 nm
90.5 %

@Wavelength 630 nm
Descriptive Properties Value Comments
Color Violet
Users viewing this material also viewed the following: