Material Notes:
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG385, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG630, RG645, RG665, RG695, RG715, RG780, RG830, RG850, RG1000, WG225, WG280, WG295, WG305, WG320
Physical Properties Metric English Comments
Density 3.61 g/cc
0.130 lb/in³
Thermal Properties Metric English Comments
CTE, linear 9.10 µm/m-°C

@Temperature -30.0 - 70.0 °C
5.06 µin/in-°F

@Temperature -22.0 - 158 °F
10.6 µm/m-°C

@Temperature 20.0 - 300 °C
5.89 µin/in-°F

@Temperature 68.0 - 572 °F
Transformation Temperature, Tg 438 °C
820 °F
Glass Temperature Coefficient 0.060
0.060
Optical Properties Metric English Comments
Refractive Index 1.60

@Wavelength 1014 nm
1.60

@Wavelength 1014 nm
Hg
1.62

@Wavelength 587.6 nm
1.62

@Wavelength 587.6 nm
He
1.65

@Wavelength 404.7 nm
1.65

@Wavelength 404.7 nm
Hg
Transmission, Visible 54 %

@Wavelength 400 nm
54 %

@Wavelength 400 nm
89 %

@Wavelength 560 - 700 nm
89 %

@Wavelength 560 - 700 nm
Internal transmittance of 99% from 560-700 nm
IR Transmittance 90 %

@Wavelength 720 - 1900 nm
90 %

@Wavelength 720 - 1900 nm
Internal transmittance of 100%  from 720-1900 nm.
UV Transmittance <= 0.0010 %

@Wavelength 200 - 350 nm
<= 0.0010 %

@Wavelength 200 - 350 nm
36 %

@Wavelength 390 nm
36 %

@Wavelength 390 nm
Internal transmittance of 40% at 390 nm
Reflection Coefficient, Visible (0-1) 0.90
0.90
Chemical Properties Metric English Comments
Acid Class, SR 1
1
Alkali Class, AR 2.3
2.3
Stain Resistance Class, FR 0.0
0.0