Schott GG385 Long Pass Filter

Category Ceramic , Glass , Filter , Optical
Manufacturer Schott Glas Mainz
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Schott GG385 Long Pass Filter.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG630, RG645, RG665, RG695, RG715, RG780, RG830, RG850, RG1000, WG225, WG280, WG295, WG305, WG320
Physical Properties Metric English Comments
Density 3.22 g/cc
0.116 lb/in³
Thermal Properties Metric English Comments
CTE, linear 8.20 µm/m-°C

@Temperature -30.0 - 70.0 °C
4.56 µin/in-°F

@Temperature -22.0 - 158 °F
9.60 µm/m-°C

@Temperature 20.0 - 300 °C
5.33 µin/in-°F

@Temperature 68.0 - 572 °F
Transformation Temperature, Tg 459 °C
858 °F
Glass Temperature Coefficient 0.060
0.060
Optical Properties Metric English Comments
Refractive Index 1.56

@Wavelength 1014 nm
1.56

@Wavelength 1014 nm
Hg
1.58

@Wavelength 587.6 nm
1.58

@Wavelength 587.6 nm
He
1.60

@Wavelength 404.7 nm
1.60

@Wavelength 404.7 nm
Hg
Transmission, Visible 70 %

@Wavelength 400 nm
70 %

@Wavelength 400 nm
90 %

@Wavelength 550 - 700 nm
90 %

@Wavelength 550 - 700 nm
Internal transmittance of 99% at 570-700 nm
IR Transmittance 91 %

@Wavelength 750 - 1900 nm
91 %

@Wavelength 750 - 1900 nm
Internal transmittance of 100%  from 750-1900 nm.
UV Transmittance <= 0.30 %

@Wavelength 200 - 360 nm
<= 0.30 %

@Wavelength 200 - 360 nm
55 %

@Wavelength 390 nm
55 %

@Wavelength 390 nm
Internal transmittance of 61% at 390 nm
Reflection Coefficient, Visible (0-1) 0.92
0.92
Chemical Properties Metric English Comments
Acid Class, SR 1
1
Alkali Class, AR 1
1
Stain Resistance Class, FR 0.0
0.0