Schott G018-310 Dental Glass

Category Ceramic , Glass
Manufacturer Schott North America
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Schott G018-310 Dental Glass.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Remarks: Zr-containing, high refractive indexApplication: CompositeAdvantagesGreater variety of composition and refractive indiciesOutstanding transparencyBest radiopacitiesInformation Provided by SCHOTT North America, Inc.
Physical Properties Metric English Comments
Density 3.00 g/cc
0.108 lb/in³
Thermal Properties Metric English Comments
CTE, linear 4.50 µm/m-°C

@Temperature -30.0 - 70.0 °C
2.50 µin/in-°F

@Temperature -22.0 - 158 °F
Transformation Temperature, Tg 680 °C
1260 °F
ISO 7884-8
Optical Properties Metric English Comments
Refractive Index 1.60
1.60
n<sub>d</sub>
Component Elements Properties Metric English Comments
Al2O3 20 %
20 %
SiO2 45 %
45 %
ZrO2 5.0 %
5.0 %
Descriptive Properties Value Comments
Cs2O (%) <5
Hydrolytic Resistance Class 1
DIN ISO 719
La2O3 (%) 20
Li2O (%) <5
Radiopacity (digital method) 780
ISO 4049
Ta2O5 (%) <5
ZnO (%) <5