Material Notes:
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include BG34, FG3
Physical Properties Metric English Comments
Density 2.78 g/cc
0.100 lb/in³
Thermal Properties Metric English Comments
CTE, linear 9.60 µm/m-°C

@Temperature -30.0 - 70.0 °C
5.33 µin/in-°F

@Temperature -22.0 - 158 °F
10.5 µm/m-°C

@Temperature 20.0 - 300 °C
5.83 µin/in-°F

@Temperature 68.0 - 572 °F
Transformation Temperature, Tg 566 °C
1050 °F
Optical Properties Metric English Comments
Refractive Index 1.55

@Wavelength 706.5 nm
1.55

@Wavelength 706.5 nm
He
1.56

@Wavelength 587.6 nm
1.56

@Wavelength 587.6 nm
He
Transmission, Visible <= 2.0 %

@Wavelength 400 - 460 nm
<= 2.0 %

@Wavelength 400 - 460 nm
78 %

@Wavelength 700 nm
78 %

@Wavelength 700 nm
Internal transmittance of 86% at 700 nm.
IR Transmittance 87 - 88 %

@Wavelength 1500 - 2100 nm
87 - 88 %

@Wavelength 1500 - 2100 nm
Internal transmittance of 96-97% from 1500-2100 nm.
UV Transmittance <= 0.0010 %

@Wavelength 200 - 390 nm
<= 0.0010 %

@Wavelength 200 - 390 nm
Internal transmittance of 0.001% from 200-390 nm.
Reflection Coefficient, Visible (0-1) 0.91
0.91
Chemical Properties Metric English Comments
Acid Class, SR 3.4
3.4
Alkali Class, AR 1
1
Stain Resistance Class, FR 1
1