Schmolz + Bickenbach UGIMA® 4404HM Low Nickel Bar

Category Metal , Ferrous Metal
Manufacturer Schmolz + Bickenbach (Swiss Steel International)
Trade Name UGIMA®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Schmolz + Bickenbach UGIMA® 4404HM Low Nickel Bar.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: UGIMA® is a range of grades with improved mahcinability highly valued by users. Ugitech maintains its technological advance by launching the new generation of UGIMA®. With this range it can increase the productivity by 20 to 40%Information provided by Schmolz + Bickenbach
Component Elements Properties Metric English Comments
Carbon, C <= 0.030 %
<= 0.030 %
Chromium, Cr 16.5 - 17.5 %
16.5 - 17.5 %
Copper, Cu <= 0.75 %
<= 0.75 %
Iron, Fe >= 64.15 %
>= 64.15 %
Manganese, Mn <= 2.0 %
<= 2.0 %
Molybdenum, Mo 2.0 - 2.5 %
2.0 - 2.5 %
Nickel, Ni 10 - 12 %
10 - 12 %
Phosphorous, P <= 0.040 %
<= 0.040 %
Silicon, Si <= 1.0 %
<= 1.0 %
Sulfur, S 0.020 - 0.030 %
0.020 - 0.030 %