Schmolz + Bickenbach UGIMA® 4305HM Low Nickel Bar

Category Metal , Ferrous Metal
Manufacturer Schmolz + Bickenbach (Swiss Steel International)
Trade Name UGIMA®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Schmolz + Bickenbach UGIMA® 4305HM Low Nickel Bar.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: UGIMA® is a range of grades with improved mahcinability highly valued by users. Ugitech maintains its technological advance by launching the new generation of UGIMA®. With this range you can increase your productivity by 20 to 40%Information provided by Schmolz + Bickenbach
Component Elements Properties Metric English Comments
Carbon, C <= 0.070 %
<= 0.070 %
Chromium, Cr 17 - 18 %
17 - 18 %
Copper, Cu <= 0.75 %
<= 0.75 %
Iron, Fe >= 68.04 %
>= 68.04 %
Manganese, Mn 1.5 - 2.0 %
1.5 - 2.0 %
Molybdenum, Mo <= 0.50 %
<= 0.50 %
Nickel, Ni 8.2 - 9.5 %
8.2 - 9.5 %
Phosphorous, P <= 0.040 %
<= 0.040 %
Silicon, Si <= 0.75 %
<= 0.75 %
Sulfur, S 0.25 - 0.35 %
0.25 - 0.35 %