Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Schmelzer Industries Pearlveil 110-30 Fiberglass Veil

Category Ceramic , Glass , Glass Fiber , Other Engineering Material , Composite Fibers
Manufacturer Schmelzer Industries
Trade Name Pearlveil
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Schmelzer Industries Pearlveil 110-30 Fiberglass Veil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Economical alternative for flat or shallow applications. Suitable for hand lay-up, pre-form molding, press molding, vacuum molding, and injection molding. Data provided by the manufacturer, Schmelzer Industries.
Mechanical Properties Metric English Comments
Hardness, Barcol 29
29
Tensile Strength, Ultimate 19.91 MPa
2888 psi
s.d. 1.47 MPa, test specimen 1.21 cm wide (s.d. 0.005 cm), 0.20 cm thick (s.d. 0.013 cm)
Elongation at Break 0.48 %
0.48 %
Elongation at max. load, 0.48%
Modulus of Elasticity 4.78 GPa
693 ksi
std. dev. 0.83 GPa
Flexural Strength 38.99 MPa
5655 psi
s.d. 1.29 MPa, specimen 2.47 cm wide (s.d. 0.02 cm), 0.20 cm thick (s.d.008 cm), 3.8 cm span (s.d. 0 cm). Test conditions: Humidity 50%, Temp. 23°C.
Flexural Modulus 3.30 GPa
479 ksi
Tangent