Schmelzer Industries Pearlveil 110-15 Fiberglass Veil

Category Ceramic , Glass , Glass Fiber , Other Engineering Material , Composite Fibers
Manufacturer Schmelzer Industries
Trade Name Pearlveil
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Schmelzer Industries Pearlveil 110-15 Fiberglass Veil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Economical alternative for flat or shallow applications. Suitable for hand lay-up, pre-form molding, press molding, vacuum molding, and injection molding. Data provided by the manufacturer, Schmelzer Industries.
Mechanical Properties Metric English Comments
Hardness, Barcol 32
32
Tensile Strength, Ultimate 26.97 MPa
3912 psi
s.d. 1.31 MPa, test specimen 1.22 cm wide (s.d. 0.003 cm), 0.23 cm thick (s.d. 0.005 cm)
Elongation at Break 0.66 %
0.66 %
Elongation at max. load, 0.65%
Modulus of Elasticity 4.76 GPa
690 ksi
std. dev. 0.12 GPa
Flexural Strength 55.9 MPa
8110 psi
s.d. 6.1 MPa, specimen 2.49 cm wide (s.d. 0.02 cm), 0.21 cm thick (s.d.01 cm), 3.8 cm span (s.d. 0 cm). Test conditions: Humidity 50%, Temp. 23°C.
Flexural Modulus 4.00 GPa
580 ksi
Tangent