Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Sax Polymers SAXLAC 320 Acrylonitrile Butadiene Styrene

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
Manufacturer Sax Polymers
Trade Name SAXLAC
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sax Polymers SAXLAC 320 Acrylonitrile Butadiene Styrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Saxalac 320 is a high impact resistant, easy flowing ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.Information provided by SAX Polymers
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
Melt Flow 20 g/10 min

@Load 10.0 kg,
Temperature 220 °C
20 g/10 min

@Load 22.0 lb,
Temperature 428 °F
from MVR; ISO 1033
Mechanical Properties Metric English Comments
Tensile Strength 42.0 MPa
6090 psi
ISO 527-1
Elongation at Break 7.0 %
7.0 %
ISO 527-1
Tensile Modulus 2.20 GPa
319 ksi
ISO 527-1
Izod Impact, Notched (ISO) 10.0 kJ/m²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
25.0 kJ/m²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Izod Impact, Unnotched (ISO) 100 kJ/m²

@Temperature 23.0 °C
47.6 ft-lb/in²

@Temperature 73.4 °F
ISO 180
100 kJ/m²

@Temperature -30.0 °C
47.6 ft-lb/in²

@Temperature -22.0 °F
ISO 180
Charpy Impact Unnotched 10.0 J/cm²

@Temperature 23.0 °C
47.6 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
10.0 J/cm²

@Temperature -30.0 °C
47.6 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
2.40 J/cm²

@Temperature 23.0 °C
11.4 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Hot Ball Pressure Test 95.0 °C

@Thickness 2.00 mm
203 °F

@Thickness 0.0787 in
IE/CEN 60335-1
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °C
180 °F
80*10*4 s=60mm; ISO 75-1 a
Vicat Softening Point 95.0 °C
203 °F
50B; ISO 306
Flammability, UL94 HB
HB
Glow Wire Test 650 °C
1200 °F
IE/CEN 60695-2-12
Processing Properties Metric English Comments
Melt Temperature 220 - 260 °C
428 - 500 °F
Mold Temperature 60.0 - 90.0 °C
140 - 194 °F
Drying Temperature 80.0 °C

@Time 7200 - 14400 sec
176 °F

@Time 2.00 - 4.00 hour
Moisture Content <= 0.20 %
<= 0.20 %