Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samyang Tripet® 2550GN45 Polyethylene Terephthalate, 45% Glass Fiber Reinforced, Flame Retardant  (discontinue.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TRIPET® has excellent heat resistance, good surface, chemical resistance and high electrical performance.Applications:Coil BobbinConnectorMotor HousingLamp HousingRelay BaseIron bodyAll information provided by Samyang
Physical Properties Metric English Comments
Specific Gravity 1.73 g/cc
1.73 g/cc
ASTM D792
Water Absorption 0.10 %

@Time 86400 sec
0.10 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm

@Thickness 3.00 mm
0.0020 - 0.0040 in/in

@Thickness 0.118 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 111
111
ASTM D785
Tensile Strength, Yield 157 MPa
22800 psi
ASTM D638
Elongation at Break 6.0 %
6.0 %
ASTM D638
Flexural Yield Strength 235 MPa
34100 psi
ASTM D790
Flexural Modulus 8.34 GPa
1210 ksi
ASTM D790
Izod Impact, Unnotched 0.834 J/cm

@Thickness 3.17 mm
1.56 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 30.0 µm/m-°C
16.7 µin/in-°F
ASTM D696
Melting Point 255 °C
491 °F
Deflection Temperature at 0.46 MPa (66 psi) 245 °C
473 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 220 °C
428 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.59 mm
V-0

@Thickness 0.0625 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Constant 3.9

@Frequency 1.00e+6 Hz
3.9

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 20.0 kV/mm
508 kV/in
ASTM D149
Dissipation Factor 0.017

@Frequency 1.00e+6 Hz
0.017

@Frequency 1.00e+6 Hz
ASTM D150
Arc Resistance 80 sec
80 sec
ASTM D495