Material Notes:
High transparency and high scratch resistance. Stable against weak acids, strong acids, weak alkalis and inorganic salts.Applications: Laptop, Monitor Front Cover - for high flow, high gloss and high hardnessInformation provided by Samyang.
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
ASTM D955
Melt Flow 8.0 g/10 min
8.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 73.5 MPa
10700 psi
ASTM D638
Elongation at Break 20 %
20 %
ASTM D638
Flexural Yield Strength 95.1 MPa
13800 psi
ASTM D790
Flexural Modulus 2.40 GPa
348 ksi
ASTM D790
Izod Impact, Notched 0.235 J/cm

@Thickness 3.17 mm
0.441 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 83.0 °C
181 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified