Samyang Triloy® S460G15 Polymer Alloy, Reinforced

Category Polymer , Thermoplastic
Manufacturer Samyang
Trade Name Triloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samyang Triloy® S460G15 Polymer Alloy, Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent impact, formability and weather resistance.220 is a reinforced grade.Applications: LCD Panel Frame - for dimensional stabilityInformation provided by Samyang.
Physical Properties Metric English Comments
Specific Gravity 1.29 g/cc
1.29 g/cc
ASTM D792
Water Absorption 0.15 %
0.15 %
ASTM D570
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
ASTM D955
Melt Flow 20 g/10 min

@Load 3.80 kg,
Temperature 250 °C
20 g/10 min

@Load 8.38 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength 83.4 MPa
12100 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Yield Strength 98.1 MPa
14200 psi
ASTM D790
Flexural Modulus 3.43 GPa
498 ksi
ASTM D790
Izod Impact, Notched 0.490 J/cm

@Thickness 3.17 mm
0.918 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 83.0 µm/m-°C
46.1 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 125 °C
257 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in
Electrical Properties Metric English Comments
Volume Resistivity 3.00e+16 ohm-cm
3.00e+16 ohm-cm
ASTM D257
Dielectric Constant 3.0
3.0
ASTM D150
Dielectric Strength 23.0 kV/mm
584 kV/in
ASTM D149
Dissipation Factor 0.0090
0.0090
ASTM D150
Arc Resistance 121 sec
121 sec
ASTM D495