Samyang Triel® 5350 Thermoplastics Polyetherester Elastomer, General Extrusion

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester, TP , Polyether Ester Elastomer
Manufacturer Samyang
Trade Name Triel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samyang Triel® 5350 Thermoplastics Polyetherester Elastomer, General Extrusion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5350 is an extrusion grade.Applications: Elastic threadInformation provided by Samyang.
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
ASTM D792
Water Absorption 0.50 %
0.50 %
ASTM D570
Linear Mold Shrinkage 0.015 - 0.017 cm/cm
0.015 - 0.017 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore D 35
35
ASTM D2240
Tensile Strength, Ultimate 14.7 MPa
2130 psi
ASTM D638
Tensile Strength, Yield 4.41 MPa

@Strain 5.00 %
640 psi

@Strain 5.00 %
ASTM D638
5.88 MPa

@Strain 10.0 %
853 psi

@Strain 10.0 %
ASTM D638
8.34 MPa

@Strain 50.0 %
1210 psi

@Strain 50.0 %
ASTM D638
Izod Impact, Notched NB

@Thickness 3.17 mm,
Temperature -40.0 °C
NB

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
NB

@Thickness 3.17 mm,
Temperature 23.0 °C
NB

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Descriptive Properties Value Comments
Flexible Rate > 400%
ASTM D638