Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Samyang Triel® 5302FR Thermoplastics Polyetherester Elastomer, Non-Halogen Flame Retardancy

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester, TP , Polyether Ester Elastomer
Manufacturer Samyang
Trade Name Triel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samyang Triel® 5302FR Thermoplastics Polyetherester Elastomer, Non-Halogen Flame Retardancy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5302FR is a non-halogen, flame retardant grade.Information provided by Samyang.
Physical Properties Metric English Comments
Specific Gravity 1.17 g/cc
1.17 g/cc
ASTM D792
Water Absorption 0.50 %
0.50 %
ASTM D570
Linear Mold Shrinkage 0.015 - 0.017 cm/cm
0.015 - 0.017 in/in
ASTM D955
Melt Flow 30 - 33 g/10 min

@Load 2.16 kg,
Temperature 230 °C
30 - 33 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 30
30
ASTM D2240
Tensile Strength, Ultimate 12.3 MPa
1780 psi
ASTM D638
Flexural Yield Strength 2.26 MPa
327 psi
ASTM D790
Flexural Modulus 0.0275 GPa
3.98 ksi
ASTM D790
Izod Impact, Notched NB

@Thickness 3.17 mm,
Temperature -40.0 °C
NB

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
NB

@Thickness 3.17 mm,
Temperature 23.0 °C
NB

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 180 °C
356 °F
ASTM D2117
Vicat Softening Point 90.0 °C
194 °F
ASTM D1525
Descriptive Properties Value Comments
Flexible Rate > 400%
ASTM D638