Samyang Triel® 5206SP Thermoplastics Polyetherester Elastomer, Double Extrusion

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester, TP , Polyether Ester Elastomer
Manufacturer Samyang
Trade Name Triel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samyang Triel® 5206SP Thermoplastics Polyetherester Elastomer, Double Extrusion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5206SP is intended for double extrusion.Information provided by Samyang.
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
Water Absorption 0.50 %
0.50 %
ASTM D570
Linear Mold Shrinkage 0.015 - 0.017 cm/cm
0.015 - 0.017 in/in
ASTM D955
Melt Flow 6.0 - 10 g/10 min

@Load 2.16 kg,
Temperature 230 °C
6.0 - 10 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 20
20
ASTM D2240
Izod Impact, Notched NB

@Thickness 3.17 mm,
Temperature -40.0 °C
NB

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
NB

@Thickness 3.17 mm,
Temperature 23.0 °C
NB

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 178 °C
352 °F
ASTM D2117
Vicat Softening Point 65.0 °C
149 °F
ASTM D1525
Descriptive Properties Value Comments
Flexible Rate > 400%
ASTM D638