Material Notes:
Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1551GN30 is an impact grade.Information provided by Samyang.
Physical Properties Metric English Comments
Specific Gravity 1.59 g/cc
1.59 g/cc
ASTM D792
Water Absorption 0.070 %
0.070 %
ASTM D570
Linear Mold Shrinkage 0.0020 - 0.012 cm/cm
0.0020 - 0.012 in/in
ASTM D955
Melt Flow 40 g/10 min

@Load 2.16 kg,
Temperature 250 °C
40 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength 118 MPa
17100 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Yield Strength 167 MPa
24200 psi
ASTM D790
Flexural Modulus 7.35 GPa
1070 ksi
ASTM D790
Izod Impact, Notched 0.588 J/cm

@Thickness 3.17 mm
1.10 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 30.0 µm/m-°C
16.7 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 225 °C
437 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 0.750 mm
V-0

@Thickness 0.0295 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Constant 3.2
3.2
ASTM D150
Dielectric Strength 20.0 kV/mm
508 kV/in
ASTM D149
Dissipation Factor 0.016
0.016
ASTM D150
Arc Resistance 110 sec
110 sec
ASTM D495
Users viewing this material also viewed the following: