Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
Manufacturer Samsung, Cheil Industries
Trade Name Starex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Starex® VE-0855YS ABS, Unreinforced FR.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flame-retardant ABS that can be used in the exterior of monitorsInformation provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0020 - 0.0060 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0060 in/in

@Thickness 0.126 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0020 - 0.0060 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0060 in/in

@Thickness 0.126 in
ASTM D955
Melt Flow 6.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
6.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ASTM D785
Tensile Strength, Yield 29.4 MPa
4270 psi
5 mm/min; ASTM D638
Flexural Strength 48.1 MPa
6980 psi
2.8 mm/min; ASTM D638
Flexural Modulus 1.58 GPa
229 ksi
2.8 mm/min; ASTM D638
Izod Impact, Notched 1.27 J/cm

@Thickness 6.35 mm
2.39 ft-lb/in

@Thickness 0.250 in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 87.0 °C
189 °F
B/50; ISO R306
Flammability, UL94 5VB

@Thickness 2.50 mm
5VB

@Thickness 0.0984 in