Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Samsung Cheil Industries Infino® UF-1017S PC, Unreinforced FR

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Molded
Manufacturer Samsung, Cheil Industries
Trade Name Infino®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Infino® UF-1017S PC, Unreinforced FR.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Melt Flow 19 g/10 min

@Load 10.0 kg,
Temperature 220 °C
19 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 119
119
ASTM D785
Tensile Strength, Yield 60.8 MPa
8820 psi
50 mm/min; ASTM D638
Flexural Strength 89.2 MPa
12900 psi
2.8 mm/min; ASTM D638
Flexural Modulus 2.30 GPa
334 ksi
2.8 mm/min; ASTM D638
Izod Impact, Notched 6.37 J/cm

@Thickness 3.17 mm
11.9 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 109 °C
228 °F
B/50; ISO R306
Flammability, UL94 V-2

@Thickness 0.400 mm
V-2

@Thickness 0.0157 in
V-0

@Thickness 0.700 mm
V-0

@Thickness 0.0276 in
Users viewing this material also viewed the following: