Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Samsung Cheil Industries Infino® TK-2046H PCT, Glass Filled

Category Polymer , Thermoplastic , Polyester, TP , Polycyclohexylenedimethylene Terephthalate (PCT)
Manufacturer Samsung, Cheil Industries
Trade Name Infino®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Infino® TK-2046H PCT, Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.60 g/cc
1.60 g/cc
ASTM D792
Melt Flow 60 g/10 min

@Load 1.20 kg,
Temperature 300 °C
60 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 61.8 MPa
8960 psi
5 mm/min; ASTM D638
Flexural Strength 80.4 MPa
11700 psi
2.8 mm/min; ASTM D790
Flexural Modulus 6.96 GPa
1010 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 0.245 J/cm

@Thickness 3.17 mm
0.459 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 260 °C

@Thickness 6.40 mm
500 °F

@Thickness 0.252 in
ASTM D648
Flammability, UL94 HB

@Thickness 1.50 - 3.00 mm
HB

@Thickness 0.0591 - 0.118 in
Users viewing this material also viewed the following: