Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Samsung Cheil Industries Infino® NH-3402F PC, 40% Glass Filled FR

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 40% Glass Filled
Manufacturer Samsung, Cheil Industries
Trade Name Infino®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Infino® NH-3402F PC, 40% Glass Filled FR.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PC/GF material with 40% GF reinforcement that can be used in printer LSUInformation provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.51 g/cc
1.51 g/cc
ASTM D792
Water Absorption 0.15 %

@Temperature 23.0 °C
0.15 %

@Temperature 73.4 °F
ASTM D570
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm

@Thickness 3.20 mm
0.0010 - 0.0030 in/in

@Thickness 0.126 in
ASTM D955
Melt Flow 33 g/10 min

@Load 10.0 kg,
Temperature 250 °C
33 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 122
122
ASTM D785
Tensile Strength, Yield 140 MPa
20300 psi
5 mm/min; ASTM D638
Flexural Strength 177 MPa
25700 psi
2.8 mm/min; ASTM D790
Flexural Modulus 10.8 GPa
1560 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 1.08 J/cm

@Thickness 3.17 mm
2.02 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 110 °C

@Thickness 6.40 mm
230 °F

@Thickness 0.252 in
ASTM D648
Flammability, UL94 V-1

@Thickness 2.00 mm
V-1

@Thickness 0.0787 in
V-0

@Thickness 2.50 - 3.00 mm
V-0

@Thickness 0.0984 - 0.118 in