Samsung Cheil Industries Infino® NH-3208GL PC, Glass Filled FR

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 10% Glass Filled
Manufacturer Samsung, Cheil Industries
Trade Name Infino®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Infino® NH-3208GL PC, Glass Filled FR.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.34 g/cc
1.34 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0040 in/in

@Thickness 0.126 in
ASTM D955
Melt Flow 24 g/10 min

@Load 10.0 kg,
Temperature 220 °C
24 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 91
91
ASTM D785
Tensile Strength, Yield 105 MPa
15200 psi
5 mm/min; ASTM D638
Flexural Strength 137 MPa
19900 psi
2.8 mm/min; ASTM D790
Flexural Modulus 5.82 GPa
843 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 0.883 J/cm

@Thickness 3.17 mm
1.65 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 92.8 °C

@Thickness 6.40 mm
199 °F

@Thickness 0.252 in
ASTM D648
Vicat Softening Point 100 °C
212 °F
B/50; ISO R306
Flammability, UL94 V-0

@Thickness 0.750 mm
V-0

@Thickness 0.0295 in