Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer Samsung, Cheil Industries
Trade Name Infino®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Infino® NF-3017 PC/ABS, Unreinforced FR.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flame-retardant scratch resistant material that can be used in notebook B partInformation provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
ASTM D792
Melt Flow 21 g/10 min

@Load 2.16 kg,
Temperature 250 °C
21 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Yield 63.7 MPa
9250 psi
50 mm/min; ASTM D638
Flexural Strength 88.3 MPa
12800 psi
2.8 mm/min; ASTM D790
Flexural Modulus 2.45 GPa
356 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 0.490 J/cm

@Thickness 3.17 mm
0.918 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Flammability, UL94 V-0

@Thickness 1.00 mm
V-0

@Thickness 0.0394 in