Samsung Cheil Industries Infino® LS-3302A PC, Glass Filled High Impact

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 10% Glass Filled
Manufacturer Samsung, Cheil Industries
Trade Name Infino®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Infino® LS-3302A PC, Glass Filled High Impact.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.41 g/cc
1.41 g/cc
ASTM D792
Melt Flow 25 g/10 min

@Load 10.0 kg,
Temperature 250 °C
25 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 98.1 MPa
14200 psi
5 mm/min; ASTM D638
Flexural Strength 137 MPa
19900 psi
2.8 mm/min; ASTM D790
Flexural Modulus 5.79 GPa
839 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 1.47 J/cm

@Thickness 3.17 mm
2.76 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 148 °C
298 °F
B/50; ISO R306