Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Samsung Cheil Industries Infino® LS-1150G PC/ABS, 15% Glass Filled FR

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Glass Fiber Filled , Polycarbonate (PC)
Manufacturer Samsung, Cheil Industries
Trade Name Infino®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Infino® LS-1150G PC/ABS, 15% Glass Filled FR.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
15% GF reinforcement; can be used in mold frames for LCD BLU.Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.28 g/cc
1.28 g/cc
ASTM D792
Melt Flow 24 g/10 min

@Load 10.0 kg,
Temperature 250 °C
24 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 88.3 MPa
12800 psi
5 mm/min; ASTM D638
Flexural Strength 137 MPa
19900 psi
2.8 mm/min; ASTM D790
Flexural Modulus 4.51 GPa
654 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 0.883 J/cm

@Thickness 3.17 mm
1.65 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 127 °C

@Thickness 6.40 mm
261 °F

@Thickness 0.252 in
ASTM D648
Vicat Softening Point 128 °C
262 °F
B/50; ISO R306
Flammability, UL94 V-2

@Thickness 0.800 - 3.00 mm
V-2

@Thickness 0.0315 - 0.118 in
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved