Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Saint-Gobain Tygon® S3™ B-44-3 Bio-based Beverage Tubing Formulation

Category Polymer , Renewable/Recycled Polymer , Thermoplastic
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name Tygon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Tygon® S3™ B-44-3 Bio-based Beverage Tubing Formulation.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Tygon S3â„¢ B-44-3, from Saint-Gobain Performance Plastics, is now phthalate-free. Saint-Gobain is proud to be among the first companies to offer sustainable flexible tubing products. The bio-based Tygon S3â„¢ line combines the high performance standards customers demand with an eco-friendly tubing design. Tygon S3â„¢ Beverage Tubing is specially formulated for transferring a wide variety of beverages including soft drinks, fruit juices, flavored teas and bottled water. In virtually all cases, Tygon S3â„¢ Beverage Tubing will not affect the taste or odor of product transferred through it, while its excellent non-wetting properties facilitate complete drainage and permit simple flush-cleaning. Many of the properties inherent to Tygon S3â„¢ Beverage Tubing also apply to a wide variety of complex applications ranging from fine cosmetic production to the dispensing of water-based printing inks found in the publishing industry. The versatility and proven performance of Tygon S3â„¢ Beverage Tubing have made it a widely specified clear, flexible plastic tubing. Features and Benefits Clear as glass for easy visual monitoring of flow Lightweight and flexible for easy, quick installation Broad chemical resistance Non-wetting properties allow easy Cleaning and complete drainage Contains no BPA or phthalates Regulatory Compliance: This product is complies with FDA, 3A, and NSF standards in the US and Reach, 1935/2004/EC, and 10/2011/EU standards in the EU.Information provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Water Absorption 0.22 %

@Temperature 22.8 °C,
Time 86400 sec
0.22 %

@Temperature 73.0 °F,
Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Shore A 66

@Time 15.0 sec
66

@Time 0.00417 hour
ASTM D2240
Tensile Strength 15.2 MPa
2200 psi
ASTM D412
Tensile Strength, Yield 9.508 MPa

@Strain 200 %
1379 psi

@Strain 200 %
Elongation at Break 390 %
390 %
ASTM D412
Tear Strength 43.8 kN/m
250 pli
ASTM D1004
Compression Set 59 %

@Temperature 70.0 °C,
Time 79200 sec
59 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395 Method B
Tensile Set 57 %
57 %
ASTM D412
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 73.9 °C
165 °F
Brittleness Temperature -35.6 °C
-32.0 °F
ASTM D746
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
Clear, but value not quantified
Compliance Properties Metric English Comments
FDA Yes
Yes
NSF Yes
Yes
Descriptive Properties Value Comments
Color Clear