Saint-Gobain Tygon® Norprene® A-60-N Drinking Water Tubing Formulation.

Category Polymer , Thermoplastic
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name Tygon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Tygon® Norprene® A-60-N Drinking Water Tubing Formulation..pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Formulated for use as drinking water tubing. Complies with FDA and NSF61 criteria.Information provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Specific Gravity 0.980 g/cc
0.980 g/cc
ASTM D792-00
Water Absorption 0.30 %

@Temperature 22.8 °C,
Time 86400 sec
0.30 %

@Temperature 73.0 °F,
Time 24.0 hour
ASTM D570-98
Mechanical Properties Metric English Comments
Hardness, Shore A 62

@Time 15.0 sec
62

@Time 0.00417 hour
ASTM D2240-00
Tensile Strength 6.55 MPa
950 psi
ASTM D412-98
Tensile Strength, Yield 6.55 MPa

@Strain 100 %
950 psi

@Strain 100 %
ASTM D412-98
Elongation at Break 420 %
420 %
ASTM D412-98
Tear Strength 21.0 kN/m
120 pli
ASTM D1004-94
Compression Set 27 %

@Temperature 70.0 °C,
Time 79200 sec
27 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395-98 Method B
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 135 °C
275 °F
Brittleness Temperature -59.4 °C
-75.0 °F
ASTM D746-98
Descriptive Properties Value Comments
Color Tan