Material Notes:
Soft and flexible, Tygon® E-1000 Non-DEHP laboratory tubing delivers the same performance in a formulation that contains non-DEHP [Bis (2-ethylhexyl) phthalate] plasticizers. The market demand and certain global and regional requirements such as Europe's REACH, EU food directives and California Prop 65 motivated Saint-Gobain to develop tubing products that contain a globally accepted substitute for DEHP. Tygon E-1000 Non-DEHP laboratory tubing has been tested rigorously to ensure that it meets the same physical standards, including low temperature and corrosive chemical resistance as the old Tygon® R-1000 tubing. Tygon® E-1000 tubing stays flexible at temperatures as low as -67°F (-55°C ). Its smooth bore facilitates easy cleaning and helps prevent possible buildup. Do not autoclave. Features and Benefits Ultra-soft and flexible Performs well at low temperatures (to -67°F) Excellent for use in low-torque pump application Regulatory Information: This product complies with NSF 51 and FDA requirements. Unless otherwise noted, all tests were conducted at room temperature. Values shown were determined on 1.9 mm thick extruded strip or 1.9 mm thick molded ASTM placques or molded ASTM durometer buttons.Information provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Water Absorption 0.29 %

@Temperature 22.8 °C,
Time 86400 sec
0.29 %

@Temperature 73.0 °F,
Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Shore A 40

@Time 15.0 sec
40

@Time 0.00417 hour
ASTM D2240
Tensile Strength 7.412 MPa
1075 psi
ASTM D412
Tensile Strength, Yield 1.97 MPa

@Strain 100 %
286 psi

@Strain 100 %
Elongation at Break 435 %
435 %
ASTM D412
Tear Strength 18.2 kN/m
104 pli
ASTM D1004
Compression Set 55 %

@Temperature 70.0 °C,
Time 79200 sec
55 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395 Method B
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 51.7 °C
125 °F
Brittleness Temperature -55.0 °C
-67.0 °F
ASTM D746
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
Clear, but value not quantified
Compliance Properties Metric English Comments
FDA Yes
Yes
NSF Yes
Yes
Descriptive Properties Value Comments
Color Clear