Saint-Gobain Rulon® AR Bearing/Seal PTFE

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Rulon® AR Bearing/Seal PTFE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Rulon® AR is somewhat more flexible than Rulon® LR, hence suitable for seals and bonded coating of slide surfaces. It has many decades of use in automotive shaft seals and fuel metering pump cups. Rulon AR has a practically universal chemical inertness like that of Rulon LR and provides long life and reliability in continuous non-lubricated service. It is capable of operating at PV values up to approximately 10,000 psi-ft/min. Higher PV values are possible for intermittent use applications.Key Attributes:Universal chemical inertnessLong life and reliability in continuous non-lubricated serviceMore flexible than Rulon® LRWorking Temperature Range: -240° to +288°C [-400° to +550°F]
Physical Properties Metric English Comments
Density 2.22 g/cc
0.0802 lb/in³
ASTM D792
Water Absorption 0.00 %

@Time 86400 sec
0.00 %

@Time 24.0 hour
Immersion
Water Absorption at Saturation 0.00 %
0.00 %
Mechanical Properties Metric English Comments
Hardness, Shore D 75
75
Tensile Strength 13.8 MPa
2000 psi
ASTM D638
Elongation at Break 175 %
175 %
ASTM D638
Compressive Yield Strength 6.89 MPa
1000 psi
Max load under tribological use
Izod Impact, Notched 3.20 J/cm
6.00 ft-lb/in
Coefficient of Friction, Dynamic 0.15 - 0.25
0.15 - 0.25
Dry vs. Steel
Coefficient of Friction, Static 0.15 - 0.25
0.15 - 0.25
Dry vs. Steel
Limiting Pressure Velocity 0.350 MPa-m/sec
9990 psi-ft/min
Max velocity is 2.0 m/s (400 fpm)
Thermal Properties Metric English Comments
Thermal Conductivity 0.331 W/m-K
2.30 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 288 °C
550 °F
Minimum Service Temperature, Air -240 °C
-400 °F
Descriptive Properties Value Comments
Color Light Maroon