Material Notes:
A conductive PTFE material that is available in tape, sheet (extruded) and rod (extruded).Information provided by distributor TriStar Plastics Corp.
Physical Properties Metric English Comments
Density 1.95 g/cc
0.0704 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Yield 34.5 MPa
5000 psi
Elongation at Break 200 %
200 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
Continuous
288 °C
550 °F
Short Term
Minimum Service Temperature, Air -240 °C
-400 °F
Embrittlement Temp