Saint-Gobain Quartzel® Fiber/Epoxy Resin Unidirectional Composite

Category Polymer , Thermoset , Epoxy , Epoxy, Molded, Glass Fiber Filler , Filled/Reinforced Thermoset
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name Quartzel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Quartzel® Fiber/Epoxy Resin Unidirectional Composite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Quartzel® fiber is produced from quartz crystal that is ground, purified, fiberized by a fusion process. It is homogeneous, non-porous, continuous, amorphous, ultra pure silica glass. It is often used as a reinforcing agent for high performance composites. Different grades and sizes of Quartzel® offer optimized compatibility with different resin systems.Information provided by Saint-Gobain Quartz PLC.
Mechanical Properties Metric English Comments
Flexural Strength 1200 MPa
174000 psi
Flexural Modulus 35.0 GPa
5080 ksi
Compressive Yield Strength 1000 MPa
145000 psi
Shear Strength 74.0 MPa
10700 psi
Interlaminar