Material Notes:
Description: Norprene® Industrial Grade Tubing, Formulation A-60-G: Norprene® Industrial Grade Tubing outperforms neoprene, EPDM and other general-purpose tubings in test after test and application after application. It will not weaken or crack after years of exposure to heat and ozone. This provides long service in a wide range of applications such as gasketing, abrasion-resistant sleeving and cable insulation. Performance formulated for on-the-job reliability, Norprene® handles temperatures from -75°F (-60°C) to 275°F (135°C), allowing the use of one material with a broad range of temperatures. It is heat sealable and can be joined without fittings. It also has excellent resistance to inorganic (acids and bases) fluids. With its outstanding flexural fatigue resistance and high temperature capability, Norprene® Industrial Grade Tubing outlasts and outperforms virtually all other general service tubings in peristaltic and vacuum pump applications. Features/Benefits:Superior weatheringAbrasion resistantOutstanding flexural fatigue resistanceWide temperature range (-75°F to 275°F)Low gas permeability versus rubber tubingOzone and UV light resistantTypical applications include Soap and Disinfectant Dispensing, Printing Ink Transfer, Caustic Dispensing, Plating and Etching Chemicals, Wastewater Sampling, Glass and Window Wash Systems, Vacuum Pumps, Cable Insulation, Abrasion Resistant Sleeving.Information provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Specific Gravity 0.980 g/cc
0.980 g/cc
ASTM D792-98
Water Absorption 0.30 %
0.30 %
24 hours at 23°C; ASTM D570-98
Mechanical Properties Metric English Comments
Hardness, Shore A 61
61
15 seconds; ASTM D2240-97
Tensile Strength, Yield 6.89 MPa
1000 psi
ASTM D412-98
Elongation at Break 375 %
375 %
ASTM D412-98
Tensile Modulus 0.00283 GPa
0.410 ksi
ASTM D412-98
300% Modulus 0.00552 GPa
0.800 ksi
ASTM D412-98
Tear Strength 21.0 kN/m
120 pli
Initial Tear Strength; ASTM D1004-94
Compression Set 27 %

@Temperature 70.0 °C
27 %

@Temperature 158 °F
Constant Deflection, for 22 hrs.; ASTM D395-98 Method B
Tensile Set 47 %
47 %
ASTM D412-98
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 135 °C
275 °F
Brittleness Temperature -59.4 °C
-75.0 °F
ASTM D746-98
Electrical Properties Metric English Comments
Dielectric Strength 21.1 kV/mm
535 kV/in
ASTM D149-97
Descriptive Properties Value Comments
Color Black