Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Saint-Gobain Furon® TR42 Thermally Conductive Acrylic Pressure-Sensitive Transfer Adhesive

Category Polymer , Adhesive , Tape , Thermoplastic , Acrylic (PMMA)
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name Furon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Furon® TR42 Thermally Conductive Acrylic Pressure-Sensitive Transfer Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: A 2 mil thermally conductive acrylic pressure-sensitive transfer adhesive. Recommended uses: Excellent for flat surface bonding and laminating to other thermally-conductive materials. Application advantages: High peel strength adhesion to minimize air entrapment; Material can be pre-attached to a heat sink or other thermally conductive material; Adverse effects of surface roughness are minimized through a highly conformable pressure-sensitive adhesive; Flame-retardant version available; Available in slit-rolls or die cut shapes. All data based on a 0.002 inch test sample. Information provided by Saint Gobain Performance Products.
Thermal Properties Metric English Comments
Thermal Conductivity 0.400 W/m-K
2.78 BTU-in/hr-ft²-°F
ASTM E1530
Maximum Service Temperature, Air 149 °C
300 °F
Minimum Service Temperature, Air -28.9 °C
-20.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 2.10e+14 ohm-cm
2.10e+14 ohm-cm
ASTM D257
Dielectric Strength 23.6 kV/mm
600 kV/in
ASTM D1000
Descriptive Properties Value Comments
Color White
Thermal Impedance @ 10 psi 0.15°C in^2/W
ASTM E1530