Saint-Gobain Chemfab® 13 Anti-Static PTFE-Coated Glass

Category Ceramic , Glass , Glass Fiber
Manufacturer Saint-Gobain Quartz PLC
Trade Name Chemfab®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Chemfab® 13 Anti-Static PTFE-Coated Glass.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Chemfab® Anti-static Series is a high quality PTFE-coated glass fabric that can be used for release sheets, belting, or other applications requiring the dissipation of static electricity. All data based on a 0.013 inch test sample. Information provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Density 2.1052 g/cc
0.076047 lb/in³
Mechanical Properties Metric English Comments
Tear Strength Test 6.0
6.0
Lbs./In. Propagation Tear Strength in fill/transverse direction
8.0
8.0
Lbs./In. for warp/longitudinal Propagation Tear Strength
Tear Strength 30.7 kN/m
175 pli
Tensile Strength (Fill)
39.4 kN/m
225 pli
Tensile Strength (Warp)
Electrical Properties Metric English Comments
Surface Resistivity per Square <= 1.00e+6 ohm
<= 1.00e+6 ohm
Descriptive Properties Value Comments
Weight (oz/yd^2) 20.5