Material Notes:
Description: Conductive silicones expand the use of our products into the electronic assembly market. By the use of special fillers, silicone can be made thermally or electrically conductive. CF1869 is a thermally-conductive coated fabric providing thin, cost-effective heat transfer capability. It is obtainable plain or with thermally-conductive pressure sensitive adhesive on one side. All data based on a 0.009 inch test sample. Information provided by Saint Gobain Performance Products.
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
ASTM D2240
Tensile Strength, Yield 75.8 MPa
11000 psi
ASTM D412
Elongation at Break <= 5.0 %
<= 5.0 %
ASTM D412
Tear Strength 17.5 kN/m
100 pli
Initial Tear Strength; ASTM D624, Die B
Thermal Properties Metric English Comments
Thermal Conductivity 0.800 W/m-K
5.55 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 204 °C
400 °F
Minimum Service Temperature, Air -62.2 °C
-80.0 °F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
ASTM D991
Dielectric Strength 13.0 kV/mm
330 kV/in
Descriptive Properties Value Comments
Color Gray
Thermal Impedance (°Cin^2/W) 0.44
ASTM E1530