Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Saint-Gobain COHRlastic® 440S Silicone Solid/Acrylic Adhesive Pressure Sensitive Tape

Category Polymer , Adhesive , Tape , Thermoset , Silicone
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name COHRlastic®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain COHRlastic® 440S Silicone Solid/Acrylic Adhesive Pressure Sensitive Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Strip-N-Stick® tape provides all the benefits of silicone rubber in an easy-to-apply, pressure-sensitive adhesive tape form. Compressible and flexible, it can conform to irregular surfaces, wrap over cylinders or be formed to produce right angles. Applications include gasketing, vibration damping, and thermal insulation. The tape reduces the need for expensive die-cut-parts--you don't pay for the center. It also eliminates the high cost of bonding and will be slit to order for 1/2" and up. 440A combines 30 durometer solid rubber with a high-adhesion acrylic adhesive for an excellent 1/32" thick gasket material. It provides high elongation and good conformability. Adhesive temperature range for Silicone PSA is -100°F to +500°F and for Acrylic PSA, -20°F to 300°F. Silicone rubber material type is solid. Adhesive type is acrylic. All data based on a 0.03125 inch test sample. Information provided by Saint Gobain Performance Products.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 4.83 MPa
700 psi
ASTM D412
Elongation at Break 650 %
650 %
ASTM D412
Compressive Strength 0.310 MPa
45.0 psi
Compression Deflection, Compressed to 75% original thickness.; ASTM D1056
Compression Set 30 %

@Temperature 100 °C
30 %

@Temperature 212 °F
Constant Deflection, Compressed 50% for 22 hrs; ASTM D1056
Descriptive Properties Value Comments
Color Light Gray