SYNTHOS Koplen® 1020 F Expandable Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Expanded Polystyrene (EPS)
Manufacturer SYNTHOS Kralupy a.s.
Trade Name Koplen®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SYNTHOS Koplen® 1020 F Expandable Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Self-Extinguishing type Koplen®.Processing Method: By water steam or hot water, the volume of the beads is increased. Foam-processing to blocks.Specific Characteristics: Flammability according to CSN EN ISO 11925-2, class E and DIN 4102-B1. Compared to type 0814F lower absorptivity and volumetric changes.Typical Application: Large-size, low density molded bolocks. Cut boards for thermal insulation of buildings and equpiment acc CSN EN 13163.Synthos was formerly known as Kaucuk. All information provided by Synthos.
Physical Properties Metric English Comments
Bulk Density 0.0150 g/cc
0.000542 lb/in³
Minimum
0.0150 - 0.0400 g/cc
0.000542 - 0.00145 lb/in³
Typical
Particle Size 1250 - 1600 µm
1250 - 1600 µm