Material Notes:
Characteristic: Good flame retardance, non-halogen, high flow properties, high impact, high heat resistance, meets the requirements of RoHs and PaHsApplications: E/E applianceInformation Provided by SPS (Guang Zhou) Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
Melt Flow 6.0 g/10 min
6.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 18.0 MPa
2610 psi
ASTM D638
Flexural Strength 25.0 MPa
3630 psi
Flexural Modulus 1.50 GPa
218 ksi
Izod Impact, Notched 0.800 J/cm
1.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 120 °C
248 °F
ASTM D648
Flammability, UL94 V-0
V-0
E253482