Material Notes:
Characteristic: Good heat stability, good toughness, no migrating, easy to process, high glossApplications: Flame-retarded PS productAppearance: Nature color particleInformation Provided by SPS (Guang Zhou) Ltd.
Thermal Properties Metric English Comments
Flammability, UL94 V-0
V-0
Processing Properties Metric English Comments
Moisture Content <= 0.10 %
<= 0.10 %
Descriptive Properties Value Comments
7001RM4/PS Ratio 1/4