Material Notes:
Characteristic: High mechanical properties, superior heat resistance, good dimensional stabilityApplications: Power tool, chassis and E/E partsInformation Provided by SPS (Guang Zhou) Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 180 MPa
26100 psi
ASTM D638
Flexural Strength 230 MPa
33400 psi
Flexural Modulus 7.20 GPa
1040 ksi
Izod Impact, Notched 1.10 J/cm
2.06 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 260 °C
500 °F
ASTM D648
Flammability, UL94 HB
HB