Material Notes:
Characteristic: Good mechanical properties and good machining propertiesApplications: Electron equipment shell, automobile assorted partsInformation Provided by SPS (Guang Zhou) Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
Melt Flow 13 g/10 min
13 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.0 MPa
7980 psi
ASTM D638
Izod Impact, Notched 6.50 J/cm
12.2 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 125 °C
257 °F
ASTM D648
Flammability, UL94 HB
HB