Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SPS Guang Zhou FILLMAâ„¢ 5002F30A Mineral Filled Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Mineral Reinforced
Manufacturer SPS Guang Zhou
Trade Name FILLMA™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SPS Guang Zhou FILLMAâ„¢ 5002F30A Mineral Filled Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Characteristic: 30%wt of French chalk filled, high rigidity, high heat resistanceApplications: Household appliance partsInformation Provided by SPS (Guang Zhou) Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
Melt Flow 12 g/10 min
12 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 32.0 MPa
4640 psi
ASTM D638
Flexural Strength 50.0 MPa
7250 psi
Flexural Modulus 3.00 GPa
435 ksi
Izod Impact, Notched 0.450 J/cm
0.843 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 138 °C
280 °F
ASTM D648
Flammability, UL94 HB
HB