Material Notes:
The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh environment. Descriptions Bars: Aluminum alloyClips: Stainless steelThreaded insert: Stainless steelStandard treatment: SurTec 650Information provided by SMAC MontBlac Groupe Technologies
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 180 - 300 °C
356 - 572 °F
Descriptive Properties Value Comments
Damping Factor 0.1 - 0.2
F, Max Dynamic 45.5 daN
46.8 mm, 45° down and out
60.0 daN
37.8 mm, left and right
70.0 daN
40.0 mm, up and down
82.5 daN
13.2 mm, up
93.0 daN
46.5 mm, down
F, Max Static 12.5 daN
10.0 mm, up and down
12.5 daN
8.8 mm, left and right
20.0 daN
8.8 mm, 45° down and out
25.0 daN
6.0 mm, down
25.0 daN
2.8 mm, up
Transmissibility at resonance 3