Material Notes:
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. UB series are used for adhesives and coating applications such as binder for magnetic tapes and inks, adhesives for shoe industries and PVC lamination, etc. UB series have good solubility to various kinds of industrial solvents and cover a wide range of solution viscosity. These special hotmelt grades can be co-extruded as an adhesive for fire hoses and converted into thin film or powder. Films are used for lamination of textiles, non-woven, plastic sheets, etc. They show good flexibility over a wide range of application temperatures. Powders are used for interlining of fiber substrates. No solvent emission occurs with these grades because they are used through hotmelt process.Information provided by SK Chemicals.
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
ASTM D2240
Tensile Strength, Ultimate 41.2 MPa
5970 psi
ASTM D412
Elongation at Break 900 %
900 %
ASTM D412
100% Modulus 0.00461 GPa
0.668 ksi
ASTM D412
300% Modulus 0.00539 GPa
0.782 ksi
ASTM D412
Tear Strength 83.4 kN/m
476 pli
ASTM D624
Thermal Properties Metric English Comments
Melting Point 69.0 °C
156 °F
ASTM D3418
Ring & Ball Softening Point 120 °C
248 °F
ASTM E28
Descriptive Properties Value Comments
Appearance Opaque Granule