SK Chemicals SKYTHANE® U1731C Magnetic Binder

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP
Manufacturer SK Chemicals
Trade Name SKYTHANE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SK Chemicals SKYTHANE® U1731C Magnetic Binder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets and FilmHoses and TubingShoe ComponentsFire HosesInformation provided by SK Chemicals.
Physical Properties Metric English Comments
Solids Content 20 %
20 %
ASTM D1259
Viscosity 3500 - 5500 cP
3500 - 5500 cP
ASTM D803
Molecular Weight 60000 g/mol
60000 g/mol
ASTM D3536
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 83.4 MPa
12100 psi
ASTM D638
Elongation at Break 400 %
400 %
ASTM D638
100% Modulus 0.009804 GPa
1.422 ksi
ASTM D638
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 15.0 °C
59.0 °F
ASTM E1356
Descriptive Properties Value Comments
Appearance Pale Yellow Liquid