Material Notes:
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical property. It is widely used for automotive parts and various industrial parts.Information provided by SK Chemicals
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
ASTM D792
Linear Mold Shrinkage 0.0025 cm/cm
0.0025 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 72
72
ASTM D2240
Hardness, Shore D 24
24
ASTM D2240
Tensile Strength, Ultimate 24.5 MPa
3560 psi
ASTM D412
Tensile Strength, Yield 2.45 MPa

@Strain 100 %
356 psi

@Strain 100 %
ASTM D412
5.39 MPa

@Strain 300 %
782 psi

@Strain 300 %
ASTM D412
Elongation at Break 950 %
950 %
ASTM D412
Resilience 55
55
by vertical rebound; ASTM D2632
Tear Strength 78.5 kN/m
448 pli
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles 23
23
H18 Wheel; 1000g load; ASTM D1044
Thermal Properties Metric English Comments
Vicat Softening Point 73.0 °C
163 °F
ASTM D1525