SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plastics to low hardness rubber. It is a kind of thermoplastic elastomer, which can be molded with general plastic mold by plasticizing at high temperature.Information provided by SK Chemicals
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
ASTM D792
Water Absorption 1.1 %
1.1 %
24 hour; ASTM D570
Linear Mold Shrinkage 0.017 cm/cm
0.017 in/in
ASTM D955
Melt Flow 18 g/10 min

@Load 2.16 kg,
Temperature 230 °C
18 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 55
55
ASTM D2240
Tensile Strength, Ultimate 29.9 MPa
4340 psi
ASTM D638
Tensile Strength, Yield 5.88 MPa

@Strain 5.00 %
853 psi

@Strain 5.00 %
ASTM D638
12.3 MPa

@Strain 10.0 %
1780 psi

@Strain 10.0 %
ASTM D638
Elongation at Break 380 %
380 %
ASTM D638
Flexural Modulus 0.206 GPa
29.9 ksi
ASTM D790
Resilience 54
54
ASTM D2632
Izod Impact, Notched 4.90 J/cm
9.18 ft-lb/in
ASTM D256
Tear Strength 145 kN/m
827 pli
ASTM D1004
Thermal Properties Metric English Comments
Melting Point 221 °C
430 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 107 °C
225 °F
ASTM D648