SK Chemicals SKYPEL G355D Special Grade Flexibility-Resistant Grade

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester, TP
Manufacturer SK Chemicals
Trade Name SKYPEL
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SK Chemicals SKYPEL G355D Special Grade Flexibility-Resistant Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plastics to low hardness rubber. It is a kind of thermoplastic elastomer, which can be molded with general plastic mold by plasticizing at high temperature.Information provided by SK Chemicals
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
ASTM D792
Melt Flow 8.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 56
56
ASTM D2240
Tensile Strength, Ultimate 49.0 MPa
7110 psi
ASTM D638
Tensile Strength, Yield 6.37 MPa

@Strain 5.00 %
925 psi

@Strain 5.00 %
ASTM D638
10.8 MPa

@Strain 10.0 %
1560 psi

@Strain 10.0 %
ASTM D638
Elongation at Break 900 %
900 %
ASTM D638
Flexural Modulus 0.206 GPa
29.9 ksi
ASTM D790
Tear Strength 165 kN/m
941 pli
ASTM D1004
Thermal Properties Metric English Comments
Melting Point 205 °C
401 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C
185 °F
ASTM D648